MICROSTRUCTURAL STUDIES AND DURABILITY OF GEOCOMPOSITES FOR THERMAL PROTECTION COATINGS OF LANDFILLS

Authors

Name Affiliation
Natalya Seraya

D.Serikbayev East Kazakhstan Technical University

Vadim Litvinov

«Proektno-ekologicheskoe byuro» LLP

Gulzhan Daumova

D.Serikbayev East Kazakhstan Technical University

Dauren Sovetkhanov

D.Serikbayev East Kazakhstan Technical University

Merey Baimurzina

D.Serikbayev East Kazakhstan Technical University

Pages:

73-86

Views:

166

Keywords:

geocomposite, low-pressure polyethylene, geotextile, microstructure, durability, scanning electron microscopy, thermal protective coating, operational properties

Abstract

The article presents the results of experimental studies to assess the durability of a geocomposite consisting of low-pressure polyethylene (HDPE) and geotextile used to shelter winter blocks of the TMO dumps of the Kounrad mine. Samples that have been in use for various periods (from one month to three years) have been studied. Microstructural studies of HDPE and geotextile surfaces were performed using a JSM-6390LV scanning electron microscope (JEOL, 2007). It has been established that microcracks and perforations form on the HDPE surface during operation, indicating gradual deformation of the material, while the geotextile structure remains intact. The results make it possible to assess the nature of the degradation of the polymer matrix of the geocomposite and confirm its high resistance to external influences under long-term operation conditions. It was also revealed that even in the presence of microdefects in the polymer part, the coating retains its functionality and continues to effectively perform thermal protection tasks.

References

  1. Litvinov, V.V., Aitekenova, D.A., Zhuravlev, I.P., Seraya, N.V., Daumova, G.K. (2023). Increasing the Duration of Dump Leaching of Copper Under Winter Conditions. Metallurgist, 67(3-4), 542-553. https://doi.org/10.1007/s11015-023-01536-x
  2. Wu, H., Yao, C., Li, C., Miao, M., Zhong, Y., Lu, Y., Liu, T. (2020). Review of application and innovation of geotextiles in geotechnical engineering. Materials, 13(7), 1774. https://doi.org/10.3390/ma13071774
  3. Carneiro, J.R., Lopes, M.d.L. (2022). Weathering of a nonwoven polypropylene geotextile: Field vs. laboratory exposure. Materials, 15, 8216. https://doi.org/10.3390/ma15228216
  4. Al-Barqawi, M., Aqel, R., Wayne, M., Titi, H., Elhajjar, R. (2021). Polymer Geogrids: A Review of Material, Design and Structure Relationships. Materials, 14, 4745. https://doi.org/10.3390/ma14164745
  5. Scholz, P., Falkenhagen, J., Wachtendorf, V., Brüll, R., Simon, F.-G. (2024). Investigation on the Durability of a Polypropylene Geotextile under Artificial Aging Scenarios. Sustainability, 16, 3559. https://doi.org/10.3390/su16093559
  6. Tanasă, F., Nechifor, M., Ignat, M.-E., Teacă, C.-A. (2022). Geotextiles - A Versatile Tool for Environmental Sensitive Applications in Geotechnical Engineering. Textiles, 2, 189-208. https://doi.org/10.3390/textiles2020011
  7. Carneiro, J.R., Lopes, M.d.L. (2022). Weathering of a nonwoven polypropylene geotextile: Field vs. laboratory exposure. Materials, 15, 8216. https://doi.org/10.3390/ma15228216
  8. Markiewicz, A., Koda, E., Kiraga, M., Wrzesiński, G., Kozanka, K., Naliwajko, M., Vaverková, M.D. (2024). Polymeric Products in Erosion Control Applications: A Review. Polymers, 16, 2490. https://doi.org/10.3390/polym16172490
  9. Lebedev, M.P., Startsev, O.V., Petrov, M.G., Kopyrin M.M. (2023). The Formation of Microcracks during Climatic Aging of Polymer-Composite Materials. Polymer Science, Series D, 16, 116–123. https://doi.org/10.1134/S199542122301015X
  10. Balla, V.K., Kate, K.H., Satyavolu, J., Singh, P., Tadimeti, J.G.D. (2019). Additive manufacturing of natural fiber reinforced polymer composites: Processing and prospects. Composites Part B: Engineering, 106956, https://doi.org/10.1016/j.compositesb.2019.106956
  11. Chubarenko, B., Domnin, D., Simon, F.-G., Scholz, P., Leitsin, V., Tovpinets, A., Karmanov, K., Esiukova, E. (2023). Change over Time in the Mechanical Properties of Geosynthetics Used in Coastal Protection in the South-Eastern Baltic. Journal of Marine Science and Engineering, 11, 113. https://doi.org/10.3390/jmse11010113
  12. Koerner, R., Hsuan, Y., Koerner, G. (2017). Lifetime predictions of exposed geotextiles and geomembranes. Geosynthetics International, 24, 198–212. https://doi.org/10.1680/jgein.16.00026
  13. Odeh, N.A., Al-Rkaby, A.H.J. (2022). Strength, Durability, and Microstructures characterization of sustainable geopolymer improved clayey soil. Case Studies in Construction Materials, 16, e00988. https://doi.org/10.1016/j.cscm.2022.e00988
  14. Jwaida, Z., Dulaimi, A., Mashaan, N., Othuman Mydin, M.A. (2023). Geopolymers: The Green Alternative to Traditional Materials for Engineering Applications. Infrastructures, 8, 98. https://doi.org/10.3390/infrastructures8060098
  15. Aparicio-Ardila, M.A., Pedroso, G.O.M., Kobelnik, M., Valentin, C.A., Luz, M.P., Silva, J.F. (2021). Evaluating the degradation of a nonwoven polypropylene geotextile exposed to natural weathering for 3 years. International Journal of Geosynthetics and Ground Engineering, 7, 69. https://doi.org/10.1007/s40891-021-00314-6
  16. Vicuña, L., Jaramillo-Fierro, X., Cuenca, P.E., Godoy-Paucar, B., Inga-Lafebre, J.D., Chavez Torres, J.L., García, J.F., Guaya, D., Febres, J.D. (2024). Evaluation of the Effectiveness of Geogrids Manufactured from Recycled Plastics for Slope Stabilization-A Case Study. Polymers, 16, 1151. https://doi.org/10.3390/polym16081151
Seraya, N., Litvinov, V., Daumova, G., Sovetkhanov, D., & Baimurzina, М. (2026). MICROSTRUCTURAL STUDIES AND DURABILITY OF GEOCOMPOSITES FOR THERMAL PROTECTION COATINGS OF LANDFILLS. EKTU Journal of Engineering Sciences, 1(1), 73-86. https://doi.org/10.51885/3134-8009_JES_2026_1_7